Jeep Grandee Cheroki + Jeep Grand Cherokee brand Cars + Settings and routine maintenance + Ryadny six-cylinder engine + V8 Engine + Procedures of the general and major maintenance of the engine + Systems of cooling, heating and air conditioning + the Power supply system and production of the fulfilled gases + System of electric equipment of the engine + Systems of decrease in toxicity of the fulfilled gases and engine management + Manual box of gear shifting + Automatic transmission + Transfer case + Coupling and transmission line + Brake system + Suspension bracket and steering - Body General information Care of a body Care of the panels of furnish made of vinyl Care of an upholstery and salon rugs Repair of insignificant damages of body panels Repair of considerable damages of a body Service of loops and locks Replacement wind and motionless glasses Removal, installation and adjustment of provision of a cowl Removal and installation of the lock of a cowl and cable of its drive Removal and installation to the place of the panel of a decorative front grille Removal and installation of a forward wing Removal and installation of bumpers Removal and installation of the panel of an internal upholstery of a door Removal, installation and adjustment of provision of a door Removal and installation of handles, cylinder and clamp (latch) of the lock of a door Removal and installation of a windowpane of a door Removal and installation of a regulator of a window of a door Removal and installation of the central console Removal and installation of the panel of an upholstery of a door of a back Removal, installation and adjustment of provision of a door of a back Replacement of an emphasis of a door of a back Removal and installation of facing of a combination of devices Removal and installation of facings of a control panel Removal and installation of a control panel Removal and installation of covers of a casing of a steering column Removal and installation of rear-view mirrors Remove also installation of a lattice of a fairing Removal and installation of seats Control body sizes + System of onboard electric equipment + Governing bodies and operation receptions
|
Repair of insignificant damages of body panels
Elimination of traces of small scratches
|
|
- If scratch superficial also does not mention panel metal, its repair is made extremely simply. For removal of particles of the lagged behind paint and a wax covering slightly rub the scratched area with thin grinding paste. Rinse the processed surface with pure water.
- Small brush paint over scratch the paint applied to an external covering of surrounding panels of a body. Continue to put paint a layer behind a layer until the surface it in scratch will not reach level of a surrounding surface of the panel. Give to new paint полимеризоваться within at least two weeks, then polish a transitional surface aflush with a surface of other panel with application of very thin grinding paste. In summary cover the processed surface with wax.
- If got through paint, having reached some metal of the panel and having caused its corrosion, it is necessary to apply other technology of repair. A penknife scrape out from scratch a poroshkoobrazny rust, then process a surface ingibitorny paint in order to avoid corrosion development in the future. A rubber or nylon applikator cover the processed damaged area with a shpaklevka of glyantsovochny type. If necessary - that is especially useful at a shpaklevka of narrow scratches - for formation of very melkodispersny paste the shpaklevka can be diluted with solvent. Before the glyantsovochny shpaklevka will harden in scratch, wrap up a finger-tip a smooth cotton fabric. Then, having moistened a finger in solvent, quickly carry out them along the puttied surface of scratch. It will make a surface slightly concave. Now, after the shpaklevka hardening, the processed scratch can be painted according to item 2 instructions above.
|
|
Repair of dents
At repair of dents by a priority there is a pulling of the deformed surface for the purpose of its removal to original level. It is not meaningful to try to achieve absolute compliance to the original is it is all the same impossible in a type of violation of internal structure of metal of the panel at blow. Optimum removal of level of the pressed surface to level approximately on 3 mm is lower than a surface of the surrounding intact site of the panel of a body. In case the dent is very superficial a pulling it at all has no sense.
|
|
- In a case when to a concave site it is possible to reach from a reverse side of the panel it is necessary to try отрихтовать a dent from within in hammer blows with soft the brisk. Tapping a dent, densely press to its face a wooden hammer for repayment of an impulse of blow in order to avoid an excessive flexure of the deformed metal of the panel.
- If the dent was formed on a two-layer site of the panel or access to it from a reverse side is impossible for any other reason, it is necessary to apply other technique of a pulling. To Nasverlita on a concave site of the panel some small openings, trying, that they appeared in the most zaglublenny areas of a dent. Then screw in openings long саморезы, having left their heads sticking out so that it was possible to grasp them nippers. Now start to extend a dent nippers for screws.
- At the following stage of processing of a dent it is necessary to remove from the damaged surface and on a site in width about 3 cm round it. This work is best of all for making by means of a wire nozzle or the shkuryashchy disk, established in an electrodrill cartridge, also manual processing by an emery paper however is not less effective. The final stage of preparation for a shpaklevaniye is the protsarapyvaniye of naked metal of a dent a screw-driver or a fragment of a file or drilling in it small openings for ensuring the maximum adhesion of a shpaklevka to a metal surface. Further it is possible to pass to performance of procedures of a shpaklevaniye and coloring.
|
|
Repair of the rusted openings and holes
|
|
- By means of shkuryashchy or the wire nozzle, clamped in a cartridge of an electrodrill remove all traces of paint from the damaged area and on a site in width about 3 cm round it. In case of lack of possibility of use of an electrodrill work can be executed not less effectively manually by an emery paper.
Whether - after removal of paint it is possible to estimate a metal damage rate corrosion and to be defined has sense to start repair or it will be more reasonable to replace the panel entirely (if it in principle is possible). New panels can be got far not so expensively as it many motorists think. Often it appears much quicker and even to establish the new panel more economically, than to make repair of extensive damages of a body.
- Remove from the damaged panel all elements of furnish of a body, except for what can serve as a reference point for a reconstruction of an original form of the deformed sites (such as facing of block headlights, etc.). By means of scissors on metal or a nozhovochny cloth remove everything pieces of metal freely dangling, poorly fixed and hopelessly damaged by corrosion, then unbend opening edges a hammer inside for the purpose of formation of deepening for a room in it a shpaklevochny material.
- By means of a metal brush remove from the damaged metal a poroshkoobrazny rust. If there is an access to a reverse side of the damaged site, process it corrosion inhibitor.
- Before the shpaklevaniye beginning the opening is necessary for muffling. It can be made a priklepyvaniye or screwing up way to the damaged site from its reverse side of a piece of a tin or having blocked an opening a wire grid.
- After opening blocking the damaged site can be puttied and painted (see Shpaklevaniye's subsection and coloring is lower).
|
|
Shpaklevaniye and coloring
|